PU Resin For High Peeling Strength Leather
品名 ARTICLE |
物性 |
特性 Characteristics |
用途 Application | ||||
粘度 万cps/25℃ Viscosity *104cps/25℃ |
固含量 Solid % |
模量 Modulus Mpa |
断裂强度 T.S Mpa |
断裂伸长率 Elongation % | |||
HX-5040 |
18-24 |
30±1 |
4.0±1 |
≥40 |
≥550 |
中软质,皮感强,耐水解6hr不裂 Middle soft, No-crack after 6hr hydrolysis resistance |
一步法、两步法太空革 Gym shoes, wet on wet method, general method |
HX-5090HA |
18-24 |
30±1 |
7.0±1.5 |
≥40 |
≥450 |
中硬质,皮感强,耐水解6hr不裂 Middle hard, No-crack after 6hr hydrolysis resistance |
一步法、两步法太空革 Gym shoes, wet on wet method, general method |
HX-060 |
14-18 |
30±1 |
5..5±1 |
≥45 |
≥550 |
耐水解12hr不裂 No-crack after 12hr hydrolysis resistance |
两步法太空革 Gym shoes, general method |
HX-3057 |
16-22 |
35±1 |
4.0±1 |
≥35 |
≥550 |
耐水解24hr表面不裂 No-crack after 24hr hydrolysis resistance |
一步法、两步法太空革 Gym shoes, wet on wet method, general method |
HX-3065 |
18-24 |
35±1 |
5.0±1 |
≥35 |
≥550 |
可压花,耐水解24hr Excellent embossing, after 24hr hydrolysis resistance,peeling |
一步法、两步法太空革 Gym shoes, wet on wet method, general method |
HX-3035 |
6-10 |
30±1 |
1.3±0.5 |
≥15 |
≥500 |
高撕裂,耐水解 High tear strength, hydrolysis resistance |
无纺布含浸 Dipping for non-woven |
HX-3930 |
8-11 |
40±1 |
3.0±1 |
≥10 |
≥500 |
高固,耐水解 High solid, good hydrolysis resistance |
无纺布含浸 Dipping for non-woven |
HX-3935 |
8-11 |
26±1 |
3.0±1 |
≥10 |
≥500 |
低固,耐水解 Low solid, good hydrolysis resistance |
无纺布含浸 Dipping for non-woven |
HX-3980 |
8-11 |
40±1 |
6.0±1 |
≥10 |
≥300 |
高固,耐水解 High solid, good hydrolysis resistance |
无纺布含浸 Dipping for non-woven |
INQUIRY THIS PRODUCT